PROJECT 2 : WEEK 10

PROJECT 2 WEEK 10


GOOD DAY EVERYBODY! 
This week, week 10 we still working hard to do our lithography on the glass slide. The glass slide we have cut in three-part last week is to be clean now by using water-bath method.

The basic principle is based on the creation of small bubbles in the liquid. When these bubbles collapse, they emit powerful shock waves and liquid jets, among other interesting effects. Combined with liquid motion induced by acoustic streaming, the collapse of bubbles contributes to remove debris from surfaces, even when the bubbles are not in direct contact with the surface. The more bubbles that exist in a liquid being sonicated, the more cleaning effect takes place.
Figure 1: Cleaning in progress



Figure 2: An image of the machine looks

After the cleansing process, we proceed to coat our sample with photoresist,AZ 5214 by using spin coating machine as we mentioned last week, week 9.After spin coating them, we put them on a hot plate to soft bake. The soft bake temperature and the time to soft bake is fixed as constant.

Figure 3: Hotplate used to soft bake

A developer is used to develop the glass slide when the coated glass slide is shine by laser. 

Figure 4 : Developer chemical 

We immerse our sample in ethanol to stop the developing reaction. At first, we dried our sample by using hot plate, but the photoresist melt and thus cannot view the line clearly. Thus, we try to dry the sample immersed in ethanol by using Nitrogen gun. At last, the line is seen but on the other hand, the glass slide is not clear.

We try to figure out the problem and settle it. After discussion among the team, we suspect that might be the chemical problem ( developer or ethanol) or the soft bake temperature problem.

That's all from us for this Week 10. We do meet some difficulties in this week but people learn from mistake, and we do :)


Stay tuned!